Segment Bolt Corrosion: Hot-Dip Galvanizing vs Dacromet for Durable Tunnel Linings
Segment bolts are the cheapest component in a ring and the most exposed. Every joint acts as a capillary: chloride-laden groundwater, de-icing salts around metro cross-passages and stray current from traction systems all concentrate at the bolt, gasket and hand-hole interface. Once the coating breaks down, corrosion product jacks the joint open, torque relaxes and water tracks along the seam. For long-life metro and sub-sea linings, bolt protection deserves the same specification scrutiny as the precast concrete.
Hot-dip galvanizing delivers a thick, sacrificial zinc layer that tolerates abrasion well, but acid pickling carries hydrogen-embrittlement risk in high-strength bolts, and heavy zinc can disturb thread fit and torque-tension control. Dacromet-type zinc-aluminium flake coatings avoid hydrogen embrittlement, stay thin enough to preserve thread geometry and suit high-strength grades, yet offer less sacrificial reserve under severe chloride or stray-current exposure unless paired with a sealer or topcoat.
Specification tips: tie the coating system to the real exposure class rather than a generic standard, and require thickness and adhesion checks on the finished thread. Consider zinc-flake plus sealer, or duplex stainless in splash zones. On CIS hard-rock and cold-climate drives, impact damage during winter handling matters as much as chemistry — specify impact-tested coatings and sealed packing. OUSUN supplies segment bolts and TBM spares from Deyang at roughly 2–4 weeks.